Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.97 - 30.0 g/micron | 50.0 - 762 g/mil | Average value: 6.87 g/micron Grade Count:116 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Dart Drop | 0.890 - 30.0 g/micron | 22.6 - 762 g/mil | Average value: 7.88 g/micron Grade Count:55 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Dart Drop | 2.36 - 30.0 g/micron | 59.9 - 762 g/mil | Average value: 6.06 g/micron Grade Count:12 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |