Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.30 - 100 g/micron | 33.0 - 2540 g/mil | Average value: 4.92 g/micron Grade Count:158 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |