Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 7.90 g/micron | 201 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Eastman 5284 LDPE 8% EVA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, No Slip, High Antiblock, High Coefficient of FrictionApplications:Ice Ba.. |
|||
Dart Drop | 7.90 g/micron | 201 g/mil | ASTM D1709B |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Dart Drop | 7.90 g/micron | 201 g/mil | ASTM D1709B |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Dart Drop | 7.90 g/micron | 201 g/mil | ASTM D1709B |
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Dart Drop | 7.90 g/micron | 201 g/mil | ASTM D1709B |
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Dart Drop | 7.90 g/micron | 201 g/mil | ASTM D1709B |
DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |