Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Metabolix M-veraâ„¢ B5008 Film Grade Compostable Bioplastic B5008 is a compostable film product with 30% biobased carbon content that is ideal for compost bags and can liners used for organic waste diversion and for shopping and retail bags.Features:Meets re.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Westlake Elevate™ EF598 9% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Westlake Hifor LT74104 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip or antiblock. It is designed for blown film applications and is well suited for consumer an.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Westlake Hifor LT74105 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74105 is a high strength linear low density polyethylene containing medium slip and medium antiblock. It is designed for blown film applications and is well suited for.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Westlake Hifor LT74113 Hexene Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74113 is a high strength hexene linear low density polyethylene containing no slip and medium antiblock. It is designed for blown film applications and is well suited .. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Westlake Hifor LT74119 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74119 is a high strength linear low density polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applic.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Westlake Hifor LT74147 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74147 is a high strength linear low density polyethylene containing medium slip and high antiblock. It is designed for blown film applications and is well suited for c.. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Huntsman PE1201 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Good optical, medium impact strength, and good processability.Applications: Film extrusion: heavy duty packaging.FDA Notes: Conforms to FDA .. |
|||
Dart Drop | 6.69 g/micron | 170 g/mil | ASTM D1709 |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |