Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 6.563 g/micron | 166.7 g/mil | ASTM D1709 |
ExxonMobil ESCOR™ AT 320 Cast Film Resin
(discontinued **) ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical |