Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.41 g/micron | 112 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Dart Drop | 4.41 g/micron | 112 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Dart Drop | 4.41 g/micron | 112 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
Dart Drop | 4.41 g/micron | 112 g/mil | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
Dart Drop | 4.41 g/micron | 112 g/mil | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
Dart Drop | 4.41 g/micron | 112 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7120B LLDPE Blown & Cast Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |