Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 18.0 g/micron | 457 g/mil | ASTM D1709A |
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
Dart Drop | 18.0 g/micron | 457 g/mil | ASTM D1709A |
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin
(discontinued **) Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |