Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 13.8 g/micron | 351 g/mil | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Vytek™ V208C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Dart Drop | 13.8 g/micron | 351 g/mil | ASTM D1709B |
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Dart Drop | 13.8 g/micron | 350 g/mil | 26" Drop Height; ASTM D1709 |
Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform.. |