Dart Drop 13.0 g/micron
330 g/mil
F50; ASTM D1709
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Dart Drop 13.0 g/micron
330 g/mil
ASTM D1709
Huntsman PE1903 EVA Film Extrusion  (discontinued **)
9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll..
Dart Drop 13.0 g/micron
330 g/mil
ASTM D1709
ExxonMobil Escorene® LD 701.ID Blown Film Resin
Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly..
Dart Drop 13.0 g/micron
330 g/mil
ASTM D1709
ExxonMobil NTX™ NTX 101 Super Strength Film Resin
NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly..