Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 11.3 g/micron | 288 g/mil | F50; ASTM D1709 |
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and.. |
|||
Dart Drop | 11.3 g/micron @Thickness 0.0150 mm |
287 g/mil @Thickness 0.000591 in |
ASTM D1709 A |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |