Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 440 g | 440 g | ASTM D 1922 |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Elmendorf Tear Strength TD | 440 g | 440 g | ASTM D1922 |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Elmendorf Tear Strength TD | 440 g | 440 g | ASTM D1922 |
ExxonMobil Exceed™ 1518KC Metallocene Polyethylene Resin Product Description: Exceed 1518KC is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518KC have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Elmendorf Tear Strength TD | 440 g | 440 g | ASTM D1922 |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Elmendorf Tear Strength TD | 440 g | 440 g | ASTM D1922 |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Elmendorf Tear Strength TD | 440 g | 440 g | ASTM D638 |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |