Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 410 g | 410 g | Modified rectangular test specimen; ASTM D1922 |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |
|||
Elmendorf Tear Strength TD | 410 g | 410 g | ASTM D-1922 |
Bapolene® 222B Polyethylene Film Grade Bapolene 222B is a butene linear low density polyethylene for blown film applications requiring superior impact strength and toughness. It complies with US FDA 21CFR177.1520.Applications: General p.. |