Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
(discontinued **) General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Elmendorf Tear Strength TD | 110 - 690 g | 110 - 690 g | Average value: 444 g Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM-D1922 |
Braskem F2523 LDPE Blown Film Extrusion Polyethylene LDPE F2523 is a low-density polyethylene. It has good sealing characteristics, optical, and mechanical properties. It contains antiblock and slip additives. Its applications include general purpose .. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade) Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | ASTM D1922 |
ExxonMobil LDPE LD 302.56 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
Elmendorf Tear Strength TD | 110 g | 110 g | gF; ASTM D1922 |
Braskem F2523 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |