Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim.. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
LyondellBasell Petrothene® NA952000 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
LyondellBasell Petrothene® NA952094 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Elmendorf Tear Strength TD | 70 g | 70 g | ASTM D1922 |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |