Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 660 g | 660 g | ASTM D1922 |
Huntsman Rexell® L8404 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, and FDA compliant.Applications: Blown film extrusion: general purpose.Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by H.. |