Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 50 g | 50 g | ASTM D1922 |
LyondellBasell Alathon® L4907 High Density Polyethylene ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro.. |
|||
Elmendorf Tear Strength TD | 50 g | 50 g | ASTM D1922 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Elmendorf Tear Strength TD | 50 g | 50 g | ASTM D1922 |
ExxonMobil Escorene® LD-713 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App.. |