Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman 1830F Polyethylene
(discontinued **) Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman D4008-F Polyethylene
(discontinued **) Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
LyondellBasell Petrothene® NA960070 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D1922 |
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM-D1922 |
Braskem LD7000A LDPE Blown Film Extrusion Polyethylene LD7000A is a low-density polyethylene produced by the high pressure process in an autoclave reactor. It is developed for the manufacturing of extruded films. It has high mechanical and impact streng.. |
|||
Elmendorf Tear Strength TD | 130 g @Thickness 0.0381 mm |
130 g @Thickness 0.00150 in |
ASTM D-1922 |
Bapolene® 107A Low Density Polyethylene Film Extrusion Resin Bapolene® 107A is an LDPE for blown film. It contains 3400 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | ASTM D-1922 |
Bapolene® 200B Polyethylene, Film Extrusion Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an.. |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman D4052-F Polyethylene
(discontinued **) D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance... |
|||
Elmendorf Tear Strength TD | 130 g | 130 g | |
Eastman E6838-975F Polyethylene
(discontinued **) E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film.. |