Polymer Property : Tensile Strength, Ultimate = 92800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 540 - 640 MPa
78300 - 92800 psi
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 590 - 640 MPa
85600 - 92800 psi
T direction
ArcelorMittal Speed 35-440 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 560 - 640 MPa
81200 - 92800 psi
ArcelorMittal FB 560 Hot rolled ferrite-bainite steel
Available in the following: Extragal® (HDT560F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength leve..