Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.52 - 6.21 MPa | 800 - 900 psi | |
Sika Industry SikaFlex 255FC Fast Cure One Part Polyurethane Adhesive Sika 255FC SikaFlex Fast Cure One Part Polyurethane AdhesiveThis is a fast curing flexible high performance polyurethane adhesive for bonding glass to metal surfaces. Initial strength is derived fro.. |
|||
Tensile Strength, Ultimate | 5.52 - 6.21 MPa | 800 - 900 psi | |
Sika Industry SikaTack UltraFast Fast Cure One Part Polyurethane Adhesive Sika UltraFast SikaTack Fast Cure One Part Polyurethane AdhesiveThis revolutionary product uses heat instead of moisture to "pre-cure" the adhesive. The product is heated before applications using a.. |