Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 476 - 565 MPa | 69000 - 82000 psi | |
Eagle Brass 18665 MSP1, Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Ultimate | 483 - 565 MPa | 70000 - 82000 psi | |
Eagle Brass 425 Tin Brass 2%, Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Ultimate | 462 - 565 MPa | 67000 - 82000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 552 - 565 MPa | 80000 - 82000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |