Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.20 - 5.50 MPa | 174 - 798 psi | Average value: 2.39 MPa Grade Count:14 |
Overview of materials for Silicone, RTV, Construction Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values.. |