Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 16.5 - 524 MPa | 2390 - 76000 psi | Average value: 126 MPa Grade Count:190 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tensile Strength, Ultimate | 483 - 524 MPa | 70000 - 76000 psi | |
Eagle Brass 194 HSM® Copper, Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Ultimate | 421 - 524 MPa | 61000 - 76000 psi | |
Eagle Brass 519 Phosphor Bronzes 6%, 1/2 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Ultimate | 421 - 524 MPa | 61000 - 76000 psi | |
Eagle Brass 770 Nickel Silver 18%, Annealed 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |