Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 32.0 - 50.0 MPa @Temperature 60.0 - 120 °C |
4640 - 7250 psi @Temperature 140 - 248 °F |
Average value: 41.7 MPa Grade Count:1 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Tensile Strength, Ultimate | 5.00 - 50.0 MPa @Temperature 60.0 - 120 °C |
725 - 7250 psi @Temperature 140 - 248 °F |
Average value: 26.0 MPa Grade Count:1 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 30.0 - 50.0 MPa | 4350 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Tensile Strength, Ultimate | 6.89 - 50.0 MPa | 1000 - 7250 psi | Average value: 20.3 MPa Grade Count:68 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Tensile Strength, Ultimate | 35.0 - 50.0 MPa | 5080 - 7250 psi | Average value: 43.8 MPa Grade Count:16 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Ultimate | 31.0 - 50.0 MPa | 4500 - 7250 psi | Average value: 40.8 MPa Grade Count:9 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 40.0 - 50.0 MPa | 5800 - 7250 psi | ASTM D638 |
Zeus EFEP Tubing |
|||
Tensile Strength, Ultimate | 37.0 - 50.0 MPa | 5370 - 7250 psi | ASTM D638 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 35.0 - 50.0 MPa | 5080 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Tensile Strength, Ultimate | 35.0 - 50.0 MPa | 5080 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Tensile Strength, Ultimate | 35.0 - 50.0 MPa | 5080 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Tensile Strength, Ultimate | 35.0 - 50.0 MPa | 5080 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Tensile Strength, Ultimate | 30.0 - 50.0 MPa | 4350 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Tensile Strength, Ultimate | 13.0 - 50.0 MPa | 1890 - 7250 psi | Average value: 27.6 MPa Grade Count:116 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Tensile Strength, Ultimate | 33.0 - 50.0 MPa @Temperature 60.0 - 120 °C |
4790 - 7250 psi @Temperature 140 - 248 °F |
Average value: 41.0 MPa Grade Count:1 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |