Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | ASTM D638 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | Average value: 40.7 MPa Grade Count:5 |
Overview of materials for Nylon 11 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Tensile Strength, Ultimate | 41.4 - 48.3 MPa | 6000 - 7000 psi | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Tensile Strength, Ultimate | 27.6 - 48.3 MPa | 4000 - 7000 psi | |
Bulk Molding Compounds BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resis.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |
|||
Tensile Strength, Ultimate | 27.6 - 48.3 MPa | 4000 - 7000 psi | |
Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinfo.. |
|||
Tensile Strength, Ultimate | 41.4 - 48.3 MPa | 6000 - 7000 psi | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Tensile Strength, Ultimate | 41.4 - 48.3 MPa | 6000 - 7000 psi | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Tensile Strength, Ultimate | 12.4 - 48.3 MPa | 1800 - 7000 psi | Average value: 26.2 MPa Grade Count:55 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |