Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 33.0 - 39.0 MPa | 4790 - 5660 psi | Average value: 37.0 MPa Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 8.00 - 39.0 MPa | 1160 - 5660 psi | Average value: 17.0 MPa Grade Count:18 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Tensile Strength, Ultimate | 22.0 - 39.0 MPa | 3190 - 5660 psi | Average value: 31.6 MPa Grade Count:18 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 1.00 - 39.0 MPa @Temperature 50.0 - 100 °C |
145 - 5660 psi @Temperature 122 - 212 °F |
Average value: 14.6 MPa Grade Count:6 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 1.00 - 39.0 MPa @Strain 20.0 - 20.0 % |
145 - 5660 psi @Strain 20.0 - 20.0 % |
Average value: 14.6 MPa Grade Count:6 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 11.0 - 39.0 MPa | 1600 - 5660 psi | Average value: 24.5 MPa Grade Count:9 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Tensile Strength, Ultimate | 29.0 - 39.0 MPa | 4210 - 5660 psi | ISO 527 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |