Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 70.0 - 310 MPa | 10200 - 45000 psi | Average value: 173 MPa Grade Count:48 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 241 - 310 MPa | 35000 - 45000 psi | typical |
H.C. Starck NRC® 3N5 (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Tensile Strength, Ultimate | 241 - 310 MPa | 35000 - 45000 psi | typical |
H.C. Starck NRC® 4N (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Tensile Strength, Ultimate | 241 - 310 MPa | 35000 - 45000 psi | typical |
H.C. Starck NRC® 4N5 (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Tensile Strength, Ultimate | 241 - 310 MPa | 35000 - 45000 psi | typical |
H.C. Starck NRC® 5N (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Tensile Strength, Ultimate | 241 - 310 MPa @Temperature 20.0 °C |
35000 - 45000 psi @Temperature 68.0 °F |
typical |
H.C. Starck NRC® Tantalum (UNS R05200) Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di.. |
|||
Tensile Strength, Ultimate | 276 - 310 MPa | 40000 - 45000 psi | |
Eagle Brass 151 ZHC® COPPER, 1/4 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Ultimate | 250 - 310 MPa | 36300 - 45000 psi | |
ArcelorMittal 07 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC07) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Ultimate | 241 - 310 MPa | 35000 - 45000 psi | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |