Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.89 - 24.1 MPa | 1000 - 3500 psi | Reinforced |
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber) Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin.. |
|||
Tensile Strength, Ultimate | 20.7 - 24.1 MPa | 3000 - 3500 psi | TM R050-36 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Tensile Strength, Ultimate | 20.7 - 24.1 MPa | 3000 - 3500 psi | TM R050-36 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |