Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.00 - 23.0 MPa | 1020 - 3340 psi | Average value: 10.5 MPa Grade Count:8 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 8.00 - 23.0 MPa | 1160 - 3340 psi | |
ATG s.r.l. XNBR Carboxylated Nitrile Rubber |