Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 60.0 - 225 MPa @Temperature 60.0 - 230 °C |
8700 - 32600 psi @Temperature 140 - 446 °F |
Average value: 107 MPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |