Polymer Property : Tensile Strength, Ultimate = 290000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1793 - 2000 MPa
260100 - 290000 psi
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..