Polymer Property : Tensile Strength, Ultimate = 232000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1590 - 1600 MPa
230000 - 232000 psi
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel
LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi..
Tensile Strength, Ultimate 1400 - 1600 MPa
203000 - 232000 psi
SSAB Tunnplat Docol® 1400 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..