Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1060 - 1210 MPa
154000 - 175000 psi
Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 1030 - 1210 MPa
150000 - 175000 psi
Materion BrushCAST® 20C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 1030 - 1210 MPa
150000 - 175000 psi
Materion BrushCAST® 21C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 1030 - 1210 MPa
150000 - 175000 psi
Materion BrushCAST® 20CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..