Polymer Property : Tensile Strength, Ultimate = 160000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 900 - 1100 MPa
131000 - 160000 psi
After Post Sintering Heat Treatment
MarkeTech 90-7-3 Tungsten Alloy, AMS-T-21014 Class 1
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Ultimate 900 - 1100 MPa
131000 - 160000 psi
Sintered Only
MarkeTech 92-5-3 Tungsten Alloy, AMS-T-21014 Class 2
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Ultimate 900 - 1100 MPa
131000 - 160000 psi
Sintered Only
MarkeTech 93-4-3 Tungsten Alloy, AMS-T-21014 Class 2
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Ultimate 920 - 1100 MPa
133000 - 160000 psi
Sintered Only
MarkeTech 95-3-2 Tungsten Alloy, AMS-T-21014 Class 3
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Ultimate 920 - 1100 MPa
133000 - 160000 psi
Sintered Only
MarkeTech 96-3-1 Tungsten Alloy, AMS-T-21014 Class 3
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Ultimate 920 - 1100 MPa
133000 - 160000 psi
Sintered Only
MarkeTech 97-2-1 Tungsten Alloy, AMS-T-21014 Class 4
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Ultimate 1030 - 1100 MPa
150000 - 160000 psi
or higher
Universal Wire Works 4130 Steel Welding Wire
Universal 4130 is a heat treatable low alloy steel for the welding of SAE 4100 series steels. Some of these steels, the higher carbon grades, will require a preheat of 300°F to 350°F. The lower ca..
Tensile Strength, Ultimate 1000 - 1100 MPa
145000 - 160000 psi
as built, Z direction
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing
EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to ..
Tensile Strength, Ultimate 950 - 1100 MPa
138000 - 160000 psi
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Ultimate 1000 - 1100 MPa
145000 - 160000 psi
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 1000 - 1100 MPa
145000 - 160000 psi
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 951 - 1100 MPa
138000 - 160000 psi
hardened to 300 HB
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi..
Tensile Strength, Ultimate 980 - 1100 MPa
142000 - 160000 psi
ArcelorMittal Dual Phase 980 LCE Y660 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 900 - 1100 MPa
131000 - 160000 psi
Rm
Assab Steels 705M Machinery Steel
ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde..
Tensile Strength, Ultimate 980 - 1100 MPa
142000 - 160000 psi
ArcelorMittal Dual Phase 1180 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 980 - 1100 MPa
142000 - 160000 psi
ArcelorMittal Dual Phase 980 LCE Y700 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 980 - 1100 MPa
142000 - 160000 psi
ArcelorMittal Dual Phase 980 Y700 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Ultimate 940 - 1100 MPa
136000 - 160000 psi
Typical
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
Description: SUPERELSO® 890 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 890 N/mm² (130 KSI), SUPERELSO® 890 enables to make weight sav..