Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 80.0 - 94.0 MPa | 11600 - 13600 psi | |
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Strength, Ultimate | 80.0 - 94.0 MPa | 11600 - 13600 psi | |
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Strength, Ultimate | 80.0 - 94.0 MPa | 11600 - 13600 psi | |
Dow CYCLOTENE™ 3022-57 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Strength, Ultimate | 80.0 - 94.0 MPa | 11600 - 13600 psi | |
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |