Tensile Strength, Ultimate 790 - 930 MPa
115000 - 135000 psi
Materion Brush 60â„¢ 3/4 HT
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte..
Tensile Strength, Ultimate 792 - 930 MPa
115000 - 135000 psi
Ametek AM 388™ Alloy (UNS C72650) TM02
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Ultimate 792 - 930 MPa
115000 - 135000 psi
Ametek AM 388™ Alloy (UNS C72650) TM04
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..