Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 634 - 738 MPa | 92000 - 107000 psi | |
Eagle Brass 64725 MAX251C, Extra Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Tensile Strength, Ultimate | 634 - 738 MPa | 92000 - 107000 psi | |
Eagle Brass 770 Nickel Silver 18%, Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Ultimate | 680 - 740 MPa | 98600 - 107000 psi | |
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |