Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 67.6 MPa
9800 psi
ASTM D638
Plaskolite Optix® CA-82 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for injection molding and contains a mold release agent. This resin offers high heat ..
Tensile Strength, Ultimate 67.6 MPa
9800 psi
ASTM D638
Plaskolite West Optix® CA-82 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for injection molding and contains a mold release agent. This resin offers high heat ..
Tensile Strength, Ultimate 67.6 - 255 MPa
9800 - 37000 psi
Average value: 145 MPa Grade Count:28
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Tensile Strength, Ultimate 67.6 MPa
9800 psi
ASTM Data
Styron CALIBREâ„¢ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
Tensile Strength, Ultimate 67.6 MPa
9800 psi
50 mm/min; ASTM D638
Dow CALIBRE™ MEGARAD™ 2081-15 Polycarbonate
CALIBRE™ MEGARAD™ 2081-15 resin is specially formulated to meet the radiation sterilization needs of the healthcare industry, while providing exceptional clarity, heat resistance, impact strength..
Tensile Strength, Ultimate 67.6 MPa
9800 psi
Abatron AboCast/AboCure 8502-1 Epoxy
AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v..
Tensile Strength, Ultimate 67.6 - 170 MPa
9800 - 24700 psi
Average value: 141 MPa Grade Count:54
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Copyright © lookpolymers.com All Rights Reserved