Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D638 |
Plaskolite Polycarbonate Mirror Sheet Better strength, security, and flame resistance than PETG mirror sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D651 |
Resinoid 7051 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 65.0 - 131 MPa | 9430 - 19000 psi | Average value: 93.0 MPa Grade Count:3 |
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **) PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Tensile Strength, Ultimate | 65.0 - 75.0 MPa | 9430 - 10900 psi | Average value: 68.7 MPa Grade Count:16 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Ultimate | 65.0 - 197 MPa | 9430 - 28500 psi | Average value: 107 MPa Grade Count:5 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 65.0 - 342.669 MPa @Temperature -40.0 - 150 °C |
9430 - 49700.1 psi @Temperature -40.0 - 302 °F |
Average value: 128 MPa Grade Count:9 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Tensile Strength, Ultimate | 65.0 - 260 MPa @Temperature -40.0 - 150 °C |
9430 - 37700 psi @Temperature -40.0 - 302 °F |
Average value: 130 MPa Grade Count:4 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D638 |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D638 |
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D638 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D638 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527-93 |
Wellman EcoLon® MRGF1619-WBK1 Mineral and Glass Reinforced Recycled Nylon 66 Description: Post Consumer Nylon Compound; WeatherableInformation provided by Wellman. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527 |
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527 |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527 |
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | dry; ISO 527-1/-2 |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | cond; ISO 527-1/-2 |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-HXGM24 PA410-(GF+MD)30 % Glass Reinforced, % Mineral Reinforced, Heat Stabilized |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ATSM D638 |
Ashley Polymers Ashlene® 69MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced high flow Nylon 66 with exceptional dimensional stability.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ATSM D638 |
Ashley Polymers Ashlene® P252WO PPO A flame retardant resin with excellent heat deflection temperature and good impact strength.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 651 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Tensile Strength, Ultimate | 65.0 - 86.0 MPa | 9430 - 12500 psi | Average value: 80.4 MPa Grade Count:7 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | 5mm/min; ISO 527 |
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ISO 527 |
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Tensile Strength, Ultimate | 65.0 - 230 MPa @Temperature -40.0 - 200 °C |
9430 - 33400 psi @Temperature -40.0 - 392 °F |
Average value: 98.0 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | ASTM D651 |
Resinoid 7051 SS Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |