Polymer Property : Tensile Strength, Ultimate = 91700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 632 MPa
91700 psi
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Ultimate 632 MPa
91700 psi
Longitudinal
AK Steel ULTRALUME® Press Hardenable Carbon Steel
ULTRALUME Press Hardenable Steel (PHS) is AK Steel’s newest addition to our expanding product portfolio of Advanced High Strength Steels (AHSS). Aluminized Type 1 ULTRALUME PHS is intended for auto..