Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.0688 MPa @Temperature 260 °C |
880.21 psi @Temperature 500 °F |
Air Aging, 70 hours; ASTM D1414 |
Freudenberg Simrit S310 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |