Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 565 MPa | 82000 psi | |
Universal Wire Works 410 Stainless Steel Electrode Universal 410 is a 12% straight chromium electrode used for the welding of type 410 stainless steel in the fabrication of equipment that demands corrosion resistance, good strength and ductility. Al.. |
|||
Tensile Strength, Ultimate | 565 MPa | 82000 psi | |
Universal Wire Works 502 E8018-B6 Stainless Steel Electrode Universal 502 electrodes are used for the welding of types 501 and 502 straight chromium steels. Principal applications are in the fabrication of equipment for the oil and chemical industries where .. |
|||
Tensile Strength, Ultimate | 565 - 621 MPa | 82000 - 90000 psi | |
Eagle Brass 230 Red Brass, Extra Spring CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |