Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 56.4 MPa
8180 psi
Shinil Chemical SHINFLAME PC/ABS Flame Retardant Polymer TV Housing
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod..