Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5580 MPa | 810000 psi | |
Toho Tenax Besfight® G40-800 12K IMA5C EP03 Continuous Filament Carbon Fiber Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |
|||
Tensile Strength, Ultimate | 5580 MPa | 810000 psi | |
Toho Tenax Besfight® G40-800 24K IMA5C EP03 Continuous Filament Carbon Fiber Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |
|||
Tensile Strength, Ultimate | 5580 MPa | 810000 psi | |
Toho Tenax Besfight® G40-800 6K IMA-5C EP03 Continuous Filament Carbon Fiber Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |