Polymer Property : Tensile Strength, Ultimate = 79900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 551 MPa
79900 psi
Kennametal Stellite Stellite® 250
Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace..
Tensile Strength, Ultimate 551 - 620 MPa
79900 - 89900 psi
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Ultimate 551 MPa
79900 psi
ATI Allvac® Nickelvac® 400 UNS N04400 Nickel Superalloy
Nickel-Copper solid solution alloy. Uses: Equipment for mineral acids, brines, alkalis, offshore engineering, marine applications.Property values are for samples in the metallurgical condition: 165..
Tensile Strength, Ultimate 551 MPa
79900 psi
ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy
Uses: Downhole tubulars for deep, corrosive wells. Pollution control, scrubber, and radwaste systems. CPI process piping systems.Property values are for samples in the metallurgical condition: 2100°..
Tensile Strength, Ultimate 551 MPa
79900 psi
Longitudinal, Welded
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat..