Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 55.0 - 76.0 MPa | 7980 - 11000 psi | Average value: 64.3 MPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ISO 527 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 55.0 - 103 MPa | 7980 - 14900 psi | Average value: 71.5 MPa Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 50-4/AboCure 50-22 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. High-Viscosity, like molasses; Light Amber color. A structural and dielectric standard. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life: 5.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8012-3/AboCure 8012-3 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Low-viscosity, Heavy-duty, Dark Amber color. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 30 minutes.Corrosion Resistance Superior res.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-3/AboCure 8101-3 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Colorless, "Liquid glass". Superior thermal and chemical resistance, high hardness, lower exotherm permits larger castings. Shelf life is 12+ month.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-8/AboCure 8101-8 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Tar filled, low-viscosity, black, plasticized resurfacing and patching compound. Shelf life is 12+ months.Processing: Pot-life: 1-2 hrs. 1/1 ratio... |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8012-6/AboCure 8012-6 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Iron filled putty, "plastic steel". non-shrinking, adhesive filler. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio.Applications:.. |
|||
Tensile Strength, Ultimate | 55.0 - 135 MPa | 7980 - 19600 psi | Average value: 104 MPa Grade Count:15 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Tensile Strength, Ultimate | 55.0 - 82.7 MPa | 7980 - 12000 psi | Average value: 65.2 MPa Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
IDI Composites E-203 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
LyondellBasell Higlass BJ22GC Polypropylene Copolymer, 30% Glass Fiber Key Features: conventional melt flow, medium high modulus, UV-stabilized, chemically coupled, glass fiber-reinforced polypropylene copolymer, moderately high rigidity, high impact strength, excellen.. |
|||
Tensile Strength, Ultimate | 55.0 - 117 MPa | 7980 - 17000 psi | |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
Tipco Tipcolite® THD 111 Phenolic Compound, Short Glass Fibers & Minerals, Medium -Soft Flow & High Strength Medium -Soft Flow Phenolic Compound, Reinforced with Short Glass Fibres & MineralsApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, T.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
Tipco Tipcolite® VASW 150 Phenolic Compound, Glass Fibers & Minerals, Medium-Soft Flow & High Strength |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | dry; ISO 527-1/-2 |
DSM Stanyl® TC155 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D651 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D651 |
Chang Chun Plastic Longlite PM T357 Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D651 |
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | |
BASF Polystyrol® 158 K Polystyrene (Global) Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w.. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ATSM D638 |
Ashley Polymers Ashlene® PPO Resin P259 A high flow grade for applications requiring high impact strength and a high heat deflection temperature.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM data at 5 mm/min. |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ASTM D638 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | ATSM D638 |
Ashley Polymers Ashlene® PC/ABS Alloy Flame retardant alloy.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 55.0 MPa @Thickness 2.00 mm |
7980 psi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D412 |
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |