Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 550.0 MPa
79770 psi
ATI Wah Chang Infiltrated Tungsten (Copper)
Tungsten base infiltrated metal with Copper as infiltrant has been widely used in industry for years. It has proven highly advantageous because of its excellent machinability. Roughly 90% Tungsten a..