Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 54.3 MPa | 7880 psi | ASTM D638 |
Plenco 4224 Phenolic, Granular, Transfer Molded
(discontinued **) Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive ap.. |
|||
Tensile Strength, Ultimate | 54.33 MPa | 7880 psi | |
Abatron AboCast 50-11/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours.. |