Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plaskolite Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | DIN 53.504 |
Lubrizol Advanced Materials Pearlthane® Clear 15N60D Thermoplastic Polyurethane
(discontinued **) Polyester-based TPU, supplied in form of translucent, colorless or slightly yellowish pellets, combining very high hardness with excellent mechanical properties and excellent hyrdrolysis resistance... |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Transfer Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 7507 Phenolic, Granular, Compression Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ISO 527-1, 2 |
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | DIN 53504 |
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | DIN 53504 |
Lubrizol ESTANE® 5715F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 4548 Phenolic, Granular, Injection Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Toyobo T-772 Nylon, Plating Grade Key Feature: Plating grade; Glass fiber and mineral reinforced grades; thermal and impact resistantInformation provided by Toyobo Co., Ltd |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 1500 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ISO R527 |
Arkema Group Orgalloy® LE 60 HM Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ATSM D638 |
Ashley Polymers Ashlene® PC/ABS Alloy 304 General purpose high gloss with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ISO 527 |
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **) AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ASTM D638 |
Plenco 2000 Phenolic, Granular, Transfer Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Tensile Strength, Ultimate | 54.0 - 211 MPa @Temperature -40.0 - 150 °C |
7830 - 30600 psi @Temperature -40.0 - 302 °F |
Average value: 78.5 MPa Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Tensile Strength, Ultimate | 54.0 MPa | 7830 psi | ATSM D638 |
Ashley Polymers Ashlene® PC/ABS Alloy 305 General purpose high gloss with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |