Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.20 MPa
754 psi
ASTM D412
Multibase Multi-Flex® TPE G 7155 BLK
Multi-Flex® G 7155 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu..
Tensile Strength, Ultimate 5.20 MPa
754 psi
ASTM D412
Multibase Multi-Flex® TPE A 5521 BLK
TPE A 5521 is based on Shell's Kraton technology licensed to Multibase. The product is extensively used in automotive and non-automotive applications. Multi-Flex TPE contains Kratonâ„¢ G.Data p..
Tensile Strength, Ultimate 5.20 MPa
754 psi
Dow Corning SE 4422 SILICONE RTV
One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning