Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 505 MPa @Temperature 649 °C |
73200 psi @Temperature 1200 °F |
|
Haynes Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 505 MPa @Temperature 650 °C |
73200 psi @Temperature 1200 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |